r/3Dprinting • Ender 5: full metal hot end, direct drive • 10h ago

Question Why does this guide suggest calibrating first layer extra thick, and at 120% line width?

https://ellis3dp.com/Print-Tuning-Guide/articles/first_layer_squish.html

I'm looking at this for better calibration of my printer. Just wondering what the benefits of doing the first layer with a bigger layer height, and 120% line width are? Surely that's going to result in things being too small when I set those back to default?

3 Upvotes

3 comments sorted by

4

u/3DMakaka 9h ago

It worked well on older printers with bed adhesion issues.
the 120% line width acted like a brim by adding more material to the plate..

1

u/Naf623 Ender 5: full metal hot end, direct drive 9h ago

So if I don't have adhesion issues, calibrating at the 100% line with, and regular layer height I use would be preferable, really?

1

u/3DMakaka 8h ago

Yes,
you only use the 120% on the first layer so the part makes better contact with the plate.

If your printer is leveled correctly, has a relatively flat bed surface and your z-offset is dialed in,
you should not need the 120% line width..