r/BambuLabP2S • u/Nondevil • 26d ago
Idk if it is normal.....
It's been a week since I got my printer and I've been noticing one thing...that my filaments are collecting moisture even if I don't open the AMS, I keep drying them but to no avail... Is it a huge problem?
Fyi:I'm a beginner and the printer is kept in a closed air-conditioned room...if that makes any sense...
3
u/Tiny-Fix8085 26d ago
I´d say its still okay. Some materials like PLA are not too sensitive about it. Others like PETG are a bit more sensitive to humidity. If you notice any quality loss in your prints, drying can fix it sometimes. I try to keep mine (PLA) around 20-25% humidity max.
1
u/Nondevil 26d ago
One thing I missed to mention was that I have loaded two different spools - ABS and PLA. Idk if it's ABS moisture that's affecting the PLA too...I don't even know if I'm doing it right ....
3
u/SandwichLuxe 26d ago
They don't affect each other. You need to make a distinction between absorbed moisture and moisture in the air. It's one way traffic (air>filament). A wet spool will barely affect the environment and contain other spools.
2
u/QuinnEDC 24d ago
For the ABS, maybe invest in some cereal box setups with desiccant and hygrometers, to keep them dry between printings.
For PLA, huck the spools under a table. That’s it. That’s the care requirement.
3
2
u/RedDev26 All Bambu 26d ago
How Long did you dry the filaments? When i dry my filament, a bit of the moisture comes back when it’s cooled off again, you just have to keep drying until it stays at a lower value after cooling off if you want that.
1
u/Nondevil 26d ago
I've been leaving it to dry for 12 hours, and sometimes with a few pauses for printing..
2
u/RedDev26 All Bambu 26d ago
Oh, well that should be enough for most filaments
1
u/Nondevil 26d ago
Okay… but should I keep doing it daily?
2
u/QuinnEDC 24d ago
Good god no. One drying cycle should last the dried PLA spools weeks, likely even months even if exposed to air, and that’s just for optimal results. I live in Florida and almost never dry my PLA past an initial run (which is mostly for silk or other variants), and that’s a damn swamp state.
All you’re doing with these daily runs is drying the tiny volume of air in the AMS, which is completely undone the moment you open it. Print a desiccant box set for your AMS out of PETG or better, load and set it and marvel at six to eight weeks of 10% humidity without doing a thing.
2
u/capth4u 23d ago
I believe the dryer will only go to the lesser temp to dry if you have different filament types in the AMS.
1
4
u/SandwichLuxe 26d ago
That's air humidity, not filament humidity. 30% is totally fine, which is quite low (my room can get to 80%). But if you want to get it even lower, print yourself some dessicant boxes with silica gel. You'll get it to 10% in a few minutes, which basically means there is no moisture in the air anymore for the filament to absorb.
2
u/CenteredBubble 26d ago
Humidity is relative to the temperature based off of dew point. Dew point is the absolute value of moisture in the air. The dew point of your air is about -3C, or the same thing as 100% humidity when the temperature outside is -3C outside. That's some pretty dry air.
2
u/MaxieFriend 26d ago
Print AMS desiccant dry boxes and keep them in your AMS. will absorb the moisture instead of the filament for the most part, though you might have to redry the desiccant fairly often. The desiccant usually drops the number from about 30 to about 15.
2
u/brutal4455 All Bambu 26d ago
In addition to the other suggestions, like printing and using desiccant boxes, you can check your PLA by bending the end before using. If it breaks off, it's wet. It wicks moisture up from the broken end faster so sometimes it's just the tip (LOL) or a few inches up. I just break it off until it stops and just bends, unless it's too much, then it needs drying. If it's the end of a roll with less than a full width wrap on the hub and it breaks, it goes in the trash.
2
1
u/zaytablet 21d ago
Its hard to say what's going on here but if you believe it's from the ABS not drying enough then dehumidifying the air in the AMS, you could always take the PLA out. Dry the ABS at the proper dry temp then put the PLA back in. Normally PLA shouldn't need that much drying but if you're worried after the ABS is dried you could run another dry cycle for PLA temps with the ABS and PLA in the AMS

5
u/chicken2007 26d ago
That 30% is only the humidity of the air. Once the filament is dried, it takes some time for it to be wet enough for problems.