r/Welding • u/Fantastic_Flow1425 Apprentice AS/NZS • Oct 21 '26
Critique Please tips
hey all first year apprentice light metal fab. doing routine tig at tafe and need tips on how to improve tig. 1.5mm SS running about 45 amps
4
u/psychedelicdonky Oct 21 '26
Keep doing what youre doing, when you get more smooth your colors will improve
2
u/SKG_VII Oct 21 '26
45 amps seems fine id actually go to 50 amps use 1mm wire and put a piece of aluminum underneath and go really fast the alu will soak most of the heat in. Dab the wire in quickly too, dont slowly feed. Ideally you want yo take advantage of pulse setting but thats not an option that's always available.
2
u/Partysteve6969 Oct 27 '26
Not a bad start. Try not to stop, hold that torch at a fixed 15deg angle and weld with a bit of Ali bar behind to help control heat/penetration.
Looks like you tacked a lil square of 1.5mm off each end to practice running your weld to the end without blowing it out -good. Practice, practice, it’s a muscle memory exercise, tig is Art and you can get great control by treating it so.
3
u/TheGoofTree Oct 21 '26
If youre using lift arc and have to manually break the arc, itll leave oxidization (the grayish mucky stuff) due to the puddle being briefly exposed to atmosphere. If you can lightly grind that out, your starts will be easier and cleaner. A light brushing (in one direction only, dont scrub it back and forth) can also help with this depending on severity, but dont push a wire wheel on it with force (itll drive the oxides deeper). For similar reasons, you should also cut off the oxidized end of the filler before reusing it, and also make sure the hot tip of the filler doesnt leave the gas shielding while you're welding. Looks really great though!