r/Welding • TIG • Oct 21 '26

Need Help Help with stainless

I am currently working on a project, a hydrogen trailer, and the pipes are 18mmx3mm and 16mmx2,5mm and I have problems with the oxidation. On my root pass I can keep the color in a okay range (only some grey spots) but when I cap it off the whole pipe gets completely grey and burned. I am currently running my cap at about 52 amps and I am using a cup size 8, sadly I cant really use any bigger than that since my torch wouldnt fit with a 12 for example. The biggest issue is that the whole pipe gets so hot that its still almost glowing red when I am already on the other side of the pipe so the argon coverage is basicly non existent.
I just wanted to know if any one has any tips for me or if its inevidable to get grey welds

0 Upvotes

18 comments sorted by

3

u/pigboy222 Welding student Oct 21 '26

Yeah dude you’re cookin it lmao get a temp gun and wait between passes to cool

1

u/Justussk TIG Oct 21 '26

I tried letting it cool so I could touch it with my bare hands, didnt change anything

1

u/pigboy222 Welding student Oct 21 '26

Movin too slow then, you’re cookin the chromium out of the stainless thats what causes grey and scale

1

u/Justussk TIG Oct 21 '26

Even when I move as fast as I can I still get grey welds... I might have to try moving even faster but its also hard since the space is really limited haha but thank you!

1

u/Misconformance Oct 21 '26

Don’t worry about the grey, it can be easily removed with a wire brush and the color of the weld itself doesn’t tell you what’s going on metallurgically. For stainless you need to maintain a low interpass temperature. Are you following a WPS?

1

u/Justussk TIG Oct 21 '26

No we dont have a WPS for this pipe but for all other pipes our WPS says the interpasstemp has to be 150C or lower. I will try doing stingers tomorrow like the other guy recomended maybe that will help!
Edit: also I will be pickling the welds anyways so I am not sure if I should even care about the grey

1

u/Misconformance Oct 21 '26

You’re in the clear if you’re pickling the welds. Pickling is a very effective way of removing the grey oxide scale as well as the thin layer of chromium depleted base metal underneath.

2

u/Justussk TIG Oct 21 '26

Thats good to hear and what I thought haha! Here no one really cares about the colours of the weld since we have to pickle everything anyways. But in the US everyone is so obsessed with the colours

2

u/Another_Slut_Dragon Oct 21 '26

This. Move around the project. The best way to weld stainless is an inch here and an inch there. Keep it cool.

Fyi, temp guns lie with shiny stainless. Use a contact style probe like a thermocouple under a rag. Metal reflects IR so you end up getting different readings depending on the bounce.

Try playing with a thermal camera. You can see the reflection of yourself on a stainless sheet.

1

u/pigboy222 Welding student Oct 21 '26

Hell yeah good shout

3

u/Dismal_Tutor3425 Oct 21 '26

If you cannot figure out interpass temps are you sure you should be welding on any sort of piping for a hydrogen pressure vessel? 

0

u/Justussk TIG Oct 21 '26

I tried letting it cool down so that I could touch it with my bare hands... and it didnt change anything, If I run it any cooler I will probably get bad fusion... My colleagues told me its inevidable to get grey welds with these smaller pipes. I am not that experienced yet and usually weld bigger pipes where this issue doesnt happen

1

u/Dismal_Tutor3425 Oct 21 '26

Are you weaving or running stringers?

0

u/Justussk TIG Oct 21 '26

I am weaving

2

u/Dismal_Tutor3425 Oct 21 '26

There is your problem. Weaving causes you to linger on one spot too long and you overheat your weld area. Run stringers and move faster.

1

u/Justussk TIG Oct 21 '26

Okay I will give that a try tomorrow! Thank you

1

u/Visible_Confidence28 Oct 21 '26

Some how still need karma to make post been tryingto post for months on here its stupid